INColoY® alloy 825 UNS N08825/W.Nr. 2.4858
| Alọì | ohun kan | C | Si | Mn | S | Mo | Ni | Cr | Al | Ti | Fe | Cu |
| Incoloy825 | Iṣẹ́jú | 2.5 | 38.0 | 19.5 | 0.6 | 22.0 | 1.50 | |||||
| Max | 0.05 | 0.5 | 1.0 | 0.03 | 3.5 | 46.0 | 23.5 | 0.2 | 1.2 | 3.0 |
| Ipo Aolly | Agbara fifẹ Rm MpaIṣẹ́jú | Agbára ìfúnni RP 0. 2 Mpa Min | Gbigbọn 5%Iṣẹ́jú |
| ti a ti fọ | 586 | 241 | 30 |
| Ìwọ̀ng/cm3 | Aaye Iyọ℃ |
| 8.14 | 1370-1400 |
Ọpá, Pẹpẹ, Waya àti Ọjà Fífi Ṣíṣe- ASTM B 425, ASTM B 564, ASME SB 425, ASME SB 564
Àwo, ìwé àti ìlà -ASTM B 424, ASTM B 906, ASME SB 424, ASME SB 906
Píìpù àti Píìpù- ASTM B 163, ASTM B 423, ASTM B 704, ASTM B 705, ASTM B 751, ASTM B 775, ASTM B 829
Àwọn Fọ́ọ̀mù Ọjà Míràn -ASTM B 366/ASME SB 366 (Bó ṣe yẹ)
● O tayọ resistance si idinku ati oxidizing acids
● Agbara to dara si fifọ wahala-ipata
● Àìfaradà tó péye sí ìkọlù agbègbè bíi ìdènà àti ìbàjẹ́ ihò
● Ó le ko awọn acids sulfuric ati phosphoric jọra pupọ
● Awọn ohun-ini ẹrọ to dara ni yara mejeeji ati awọn iwọn otutu ti o ga titi de iwọn 1000°F
● Àṣẹ fún lílo ọkọ̀ ojú omi ní ògiri tí ó gbóná tó 800°F